Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/ProcessA/PrA-2: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
Line 76: Line 76:
| C04047.03
| C04047.03
|  
|  
[[file:C04047.03 099.jpg|150px|frameless ]]
[[file:C04047.03 100.jpg|150px|frameless ]]
[[file:C04047.03 101.jpg|150px|frameless ]]
[[file:C04047.03 102.jpg|150px|frameless ]]
[[file:C04047.03 103.jpg|150px|frameless ]]
[[file:C04047.03 104.jpg|150px|frameless ]]
[[file:C04047.03 105.jpg|150px|frameless ]]
[[file:C04047.03 106.jpg|150px|frameless ]]
[[file:C04047.03 107.jpg|150px|frameless ]]
[[file:C04047.03 108.jpg|150px|frameless ]]
[[file:C04047.03 109.jpg|150px|frameless ]]
[[file:C04047.03 097.jpg|150px|frameless ]]
[[file:C04047.03 098.jpg|150px|frameless ]]


|-
|-

Revision as of 14:43, 15 June 2016


Process runs
Date Substrate Information Process Information SEM Images
Wafer info Exposed area Conditioning Recipe Wafer ID
2/5-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-2, 80 cycles or 14:40 minutes C03991.03

2/5-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-2, 80 cycles or 14:40 minutes C03991.06

3/6-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-2, 80 cycles or 14:40 minutes C04047.03

3/6-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-2, 80 cycles or 14:40 minutes C04047.06