Specific Process Knowledge/Etch/DRIE-Pegasus/processA/PrA-0: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
Line 67: Line 67:
[[file:C03991.04 123.jpg|150px|frameless ]]
[[file:C03991.04 123.jpg|150px|frameless ]]
[[file:C03991.04 124.jpg|150px|frameless ]]
[[file:C03991.04 124.jpg|150px|frameless ]]
|-
|-
| 3/6-2016
| 3/6-2016
Line 89: Line 88:
[[file:C04047.01 073.jpg|150px|frameless ]]
[[file:C04047.01 073.jpg|150px|frameless ]]
[[file:C04047.01 074.jpg|150px|frameless ]]
[[file:C04047.01 074.jpg|150px|frameless ]]
|-
|-
| 3/6-2016
| 3/6-2016
Line 98: Line 96:
| C04047.04
| C04047.04
|  
|  
 
[[file:C04047.04 115.jpg|150px|frameless ]]
 
[[file:C04047.04 116.jpg|150px|frameless ]]
 
[[file:C04047.04 117.jpg|150px|frameless ]]
[[file:C04047.04 118.jpg|150px|frameless ]]
[[file:C04047.04 119.jpg|150px|frameless ]]
[[file:C04047.04 120.jpg|150px|frameless ]]
[[file:C04047.04 121.jpg|150px|frameless ]]
[[file:C04047.04 122.jpg|150px|frameless ]]
[[file:C04047.04 123.jpg|150px|frameless ]]
[[file:C04047.04 110.jpg|150px|frameless ]]
[[file:C04047.04 111.jpg|150px|frameless ]]
[[file:C04047.04 112.jpg|150px|frameless ]]
[[file:C04047.04 113.jpg|150px|frameless ]]
[[file:C04047.04 114.jpg|150px|frameless ]]
|-
|-
|}
|}

Revision as of 14:27, 15 June 2016


Process runs
Date Substrate Information Process Information SEM Images
Wafer info Exposed area Conditioning Recipe Wafer ID
2/5-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-0, 80 cycles or 14:40 minutes C03991.01

2/5-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-0, 80 cycles or 14:40 minutes C03991.04

3/6-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-0, 80 cycles or 14:40 minutes C04047.01

3/6-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-0, 80 cycles or 14:40 minutes C04047.04