Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
9/4-2014 4" travka05 wafer 1.5 µm AZ Si / 5 % Pegasus/jmli 5 minute TDESC clean + MU runs jml/isotropic/mediumiso1 2:00 minutes S003961 .

6/6-2016 6" travka35 wafer 1.5 µm AZ Si / 35 % Pegasus/jmli standard/danchip/mediumiso1 2:00 minutes S006534

6/6-2016 6" travka35 wafer 1.5 µm AZ Si / 35 % Pegasus/jmli standard/danchip/mediumiso1 4:00 minutes S006535