At Danchip, we have two types of bulk glass substrates: Borosilicate glass (Borofloat 33 (like pyrex)) and fused silicate glass which in cleanliness is similar to quartz. Both types are etched wet in a special set-up placed in a fumehood using a strong HF-solution (isotropic etch).
Masking materials and pre-treatment of the glass surface prior to the deposition of the masking material is a special concern in particular for deep etchings (> 10µm).
40% HF 3µm/min Beaker Maske?