Jump to content

Specific Process Knowledge/Thin film deposition/ALD Picosun R200/ALD multilayers: Difference between revisions

Eves (talk | contribs)
Eves (talk | contribs)
Line 211: Line 211:
<b>Temperature: 120 <sup>o</sup>C</b>
<b>Temperature: 120 <sup>o</sup>C</b>


All four recipes is based on <b>Al2O3_LT</b> amd <b>TiO2_LT</b> above mentioned low temperature recipes. Research based on fabricated Al<sub>2</sub>O<sub>3</sub> and TiO<sub>2</sub> multilayer has been published [http://journals.aps.org/prl/abstract/10.1103/PhysRevLett.115.177402 LINK]
All four recipes is based on <b>Al2O3_LT</b> amd <b>TiO2_LT</b> above mentioned low temperature recipes. Optical research based on fabricated Al<sub>2</sub>O<sub>3</sub> and TiO<sub>2</sub> multilayers has been published [http://journals.aps.org/prl/abstract/10.1103/PhysRevLett.115.177402 LINK]