Specific Process Knowledge/Lithography/DUVStepperLithography/Process Instructions: Difference between revisions
Created page with "The SÜSS Spinner-Stepper is dedicated for spinning DUV resists. Please note that a Bottom Anti-Reflective Coating (BARC) is necessary to guarantee high quality of both the re..." |
No edit summary |
||
| Line 1: | Line 1: | ||
== Process Instructions == | |||
The SÜSS Spinner-Stepper is dedicated for spinning DUV resists. Please note that a Bottom Anti-Reflective Coating (BARC) is necessary to guarantee high quality of both the resist film and the exposure. Please find the specification of the SÜSS Spinner-Stepper in the LabAdviser [[http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/DUVStepperLithography#SÜSS Spinner-Stepper]]. | The SÜSS Spinner-Stepper is dedicated for spinning DUV resists. Please note that a Bottom Anti-Reflective Coating (BARC) is necessary to guarantee high quality of both the resist film and the exposure. Please find the specification of the SÜSS Spinner-Stepper in the LabAdviser [[http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/DUVStepperLithography#SÜSS Spinner-Stepper]]. | ||
Revision as of 13:19, 9 May 2016
Process Instructions
The SÜSS Spinner-Stepper is dedicated for spinning DUV resists. Please note that a Bottom Anti-Reflective Coating (BARC) is necessary to guarantee high quality of both the resist film and the exposure. Please find the specification of the SÜSS Spinner-Stepper in the LabAdviser [Spinner-Stepper].
Usually, in order to guarantee the highest fidelity of the produced pattern on the wafer the best suitable exposure dose has to be evaluated for each individual pattern, resist type and resist thickness. Thus, when a new reticle is used, it is recommended to perform an exposure dose test and - for resist thicknesses larger 500 nm - additionally a focus off-set test. After evaluation by SEM the identified dose and focus - that leads to the most accurate pattern - can be applied in the DUV process for the required wafers.
The DUV process - including BARC and resist spinning, exposure, post exposure bake and development - will be performed by the customer together with the Photolith group of Danchip. Any kind of inspection, evaluation and pre- and post-processing should be performed by the customer.