==Etching of Chromium==
==Etching of Chromium==
[[Image:fumehoodetch-chrom2.jpg|300x300px|thumb|Wet Etch of Chrom in BHF in the tank placed in the fumehood: Positioned in cleanroom 2]]
[[Image:fumehoodetch-chrom.jpg|300x300px|thumb|Fume hood: positioned in cleanroom 2. <br />Wet Etch of Chromium can take place in a beaker in this fume hood]]
Etching of chromium is done wet at Danchip making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. We have two solution for this: