Line 14: Line 14:
*RCA2: 10 min
*RCA2: 10 min
*DI wafer rinsing (dumping three times)
*DI wafer rinsing (dumping three times)
*HF: 30 sec (avoid it if you have oxide as the top layer)
*Optional: HF: 30 sec (avoid it if you have oxide as the top layer)
*DI wafer rinsing (dumping three times)
*DI wafer rinsing (dumping three times)


===Overview of RCA process data===