# As mentioned before, the more experienced you are with imaging on the LEO, the more successful your patterning sessions will be. Get acquainted with the microscope software before sitting there for your exposures.
# As mentioned before, the more experienced you are with imaging on the LEO, the more successful your patterning sessions will be. Get acquainted with the microscope software before sitting there for your exposures.
# Try consulting a fully trained colleague of yours, and consider assisting him/her when she or he e-beam writes, to gather as much knowledge as possible about your desired e-beam process, e.g. which acceleration voltage, working distance, doses, are typically used.  
# Try consulting a fully trained colleague of yours, and consider assisting him/her when she or he e-beam writes, to gather as much knowledge as possible about your desired e-beam process, e.g. which acceleration voltage, working distance, doses, are typically used.  
# Study the manual for the machine, it can be found [[Specific_Process_Knowledge/Lithography/EBeamLithography/JBX9500Manual|here]]
# Study the manual for the machine, available [[Specific_Process_Knowledge/Lithography/EBeamLithography/RaithElphyManual|here]]


''' Prepare a process flow'''
''' Prepare a process flow'''
#Describe your entire process in a process flow. The process flow should include all information such as type and thickness of resist, size and type of substrate, which processes are to be done before and after e-beam writing. Find process flow templates [[Specific_Process_Knowledge/Lithography/EBeamLithography#E-beam_resists_and_Process_Flows | here]]. '''Attach your process flow to your request for training.'''
#Describe your entire process in a process flow. The process flow should include all information such as type and thickness of resist, size and type of substrate, which processes are to be done before and after e-beam writing. Find process flow templates [[Specific_Process_Knowledge/Lithography/EBeamLithography#E-beam_resists_and_Process_Flows | here]]. '''Attach your process flow to your request for training.'''
# For the Raith tool, Danchip does not provide assistance for process development. All the users are welcome to contribute to the shared knowledge by sharing their recipes, but no quality check or default recipes are available for exposures in this machine.
# For the Raith tool, Danchip expects users to perform process development by themselves. All the users are welcome to contribute to the shared knowledge by sharing their recipes, but no quality check or default recipes are available for this machine.


<br clear="all" />
<br clear="all" />

Revision as of 19:24, 14 February 2016

Feedback to this page: click here


THIS PAGE IS UNDER CONSTRUCTION

Manual

Manual for Raith Elphy

Technical Information

For an overview on the SEM imaging capabilities (often relevant during patterning as well), refer to the general SEM page.

For information regarding patterning, see comparison table here.

Getting started

  • To request an e-beam training session, contact e-beam@danchip.dtu.dk; a DTU Danchip personnel will hereafter provide a time slot. Users require 2 training sessions before being allowed full access to the machine. Please be sure to fulfill all requirements (see below) when asking for training on this equipment.
  • For other/general inquiries regarding this equipment, you can contact directly William Tiddi.


Before you request for a training on the machine, fulfill the following steps:

Be trained on the following machines:

(Contact Training to obtain missing items)

  1. SEM LEO. The Raith e-beam exposure is performed through the LEO microscope. Operating the microscope for regular imaging is always the first step in the patterning process. Being able to navigate the SEM software and to obtain high quality images will come handy to avoid spending hours without good results. If you have no previous SEM experience, you may need to be trained and get practice on a different instrument before moving to the LEO, so plan ahead.
  2. Spinner and Developer tools according to your process flow.

Create your layout:

  1. Prepare your pattern using a layout software (L-edit, CleWin, CAD) and export that to GDS format. Check your GDS-file by importing it in e.g. CleWin or L-edit.
  2. Additional functionality (e.g. single shot lines/points, dose modulation, etc.) can be obtained using directly the editor inside the Raith Elphy software. After the first training, it can be useful to prepare and/or test the layout directly in this proprietary editor.
  3. If you are unsure of the patterning parameters to use, include test structures (shape, dimension) in your layout to identify optimal parameters according to the desired resolution.

Gather Experience

  1. As mentioned before, the more experienced you are with imaging on the LEO, the more successful your patterning sessions will be. Get acquainted with the microscope software before sitting there for your exposures.
  2. Try consulting a fully trained colleague of yours, and consider assisting him/her when she or he e-beam writes, to gather as much knowledge as possible about your desired e-beam process, e.g. which acceleration voltage, working distance, doses, are typically used.
  3. Study the manual for the machine, available here

Prepare a process flow

  1. Describe your entire process in a process flow. The process flow should include all information such as type and thickness of resist, size and type of substrate, which processes are to be done before and after e-beam writing. Find process flow templates here. Attach your process flow to your request for training.
  2. For the Raith tool, Danchip expects users to perform process development by themselves. All the users are welcome to contribute to the shared knowledge by sharing their recipes, but no quality check or default recipes are available for this machine.


General Rules

For safety reasons, even fully trained users are only authorized to mount substrates into the e-beam cassettes, but not authorized to load the cassettes into the autoloader.

To use the e-beam writer, book the machine via LabManager, note the number and type of substrate as well as the condition file to be used in the 'Public Comment:' field in LabManager. Mount your substrate in the cassette and pre-align if necessary. Call for help from DTU Danchip staff to load your cassette into the robot loader (the autoloader).

After your exposure, fully trained users can unload their cassettes from the autoloader, unmount their substrates and re-load an empty cassette into the autoloader. If you are unable to unmount your substrates before another user requires the cassette, you must accept that either the next user or DTU Danchip personel unmount your substrates.

Cassettes

Some cassettes are made of Aluminum, others of Titanium. The thermal expansion coefficient of Ti is much lower than of Al; bear this in mind if you have crucial patterns to expose.

Keep an eye on the wafer orientation when you mount; the 2" aluminum cassette still have wafer orientation flat-up.


chip Al/Cu cassette with slot widths of 20 mm, 12 mm, 8 mm and 4 mm 2" Ti cassette; wafer orientation is flat-down 2" Al cassette; wafer orientation is flat-up 4" Ti cassette; wafer orientation is flat-down 4" Al cassette; wafer orientation is flat-down



Design of global marks and chip marks

If you need to align an exposure to an existing pattern on a wafer you need wafer marks (or global marks) to align your exposure to. This requires global marks and chip marks on the wafer, optimization of gain settings of backscattered electron detector (ACGRG), and execution of subprograms that detects global marks and chip marks (SETWFR and CHIPAL). The subprograms are discussed in details in the manual.

Please note that manual alignment (using the SEM) is not allowed. You should use semi-automatic alignment only. In rare cases where semi-automatic alignment is impossible, you should remove the resist around the wafer marks before loading the wafer/chip into the machine.

Definition of length and width of global mark, use L = 500-1000 µm, W 3-5 µm Text around mark is not recommended Fabricate 2 - 3 P and Q marks. Place the P marks on the left side of the wafer and Q marks to the right. Do not place the marks closer than 15 mm to the edges of the wafer. Example of chip with 4 chip marks. Always position the chip marks outside the chip pattern. Position of chip marks are entered in jdf file using chip coordinate system, i.e. center of chip is (0,0).

1 Material:

Global marks or chip marks should be clearly visible in a 100keV SEM, i.e. preferably defined by Ti/Au or another 'heavy' metal, alternatively the wafer marks should be etched. In Si, etched mark should be around 1 µm deep in order to be detectable by the machine. Shallow etched (even 200 nm etched profiles) global marks or global marks in Si or marks defined by a light metal as Al can be hard to locate manually as well as automatically by the machine.

2 Design:

  • Global marks: You need at least two wafer marks, a P mark and a Q mark. It is recommended to have many P and Q marks available on the wafer to choose from. The x-coordinate of the P mark should be smaller than the x-coordinate of the Q mark. The global marks should either be crosses or L-shaped, they should be as narrow as possible and 500 - 1000 microns in length. If the wafer contains a number of identical marks, the marks should be marked in order to identify the 'right' alignment mark (the scan width of the SEM is 1 mm x 1 mm). Text around the wafer mark is NOT recommended. Wafer marks formed as crosses with lengths of 1000 microns and 3-5 microns in width are recommended.
  • Chip marks: Prepare 1 or 4 chip marks on every chip. The chip marks can be smaller than global marks, as only very fine alignment is performed with chip marks. The chip marks should either be crosses or L-shaped and text around the marks is NOT recommended.