The laser micromachining tool is equipped with two laser sources (1) a picosecond laser (TBW) and (2) a nanosecond laser (IPG). The technical specifications provided by the supplier 3D micromac are shown below. Refer to the [[Specific_Process_Knowledge/Back-end_processing/Laser_Micromachining_Tool#Performances/|Performances]] to know the measured values. | The laser micromachining tool is equipped with two laser sources (1) a picosecond laser (TBW) and (2) a nanosecond laser (IPG). The technical specifications provided by the supplier 3D micromac are shown below. Refer to the [[Specific_Process_Knowledge/Back-end_processing/Laser_Micromachining_Tool#Performances/|Performances]] to know the measured values of the output power. | ||
=== Specifications from 3D micromac === | === Specifications from 3D micromac === | ||
Revision as of 15:22, 27 January 2016
Laser sources
The laser micromachining tool is equipped with two laser sources (1) a picosecond laser (TBW) and (2) a nanosecond laser (IPG). The technical specifications provided by the supplier 3D micromac are shown below. Refer to the Performances to know the measured values of the output power.
Specifications from 3D micromac
| Picosecond (TBW) | Nanosecond (IPG) | |
| Wavelength | 1064nm, 532nm, 355nm | 1064nm |
| Pulse duration | 10ps | 120ns |
| Repetition rate | 200 kHz up to 8000 kHz software controlled | 200kHz |
| Output power | > 50 W @ 1064 nm | 100 W |
| Warm-up time | 25min | none |