=Results for Si etching in the IBE=
=Results for Si etching in the IBE=
''Made by Kristian Hagsted Rasmussen @ Nanotech in 2011'' <br\>
''Made by Kristian Hagsted Rasmussen@Nanotech in 2011'' <br\>


The silicon etch test was made as a preliminary test of the IBE system, to obtain a felling of the system capabilities and the different parameters influence on the etch outcome. A throughout characterization of the wafers was not carried out. However, the most important results are listed here.