Is in use during the RCA procedure. | Is in use during the RCA procedure. This bath must only be used in the RCA procedure or to remove native oxide on new wafers from the box. See the [[Specific Process Knowledge/Wafer cleaning/RCA|RCA]] page for further details. | ||