Jump to content

Specific Process Knowledge/Thin film deposition/Furnace LPCVD PolySilicon/Boron doped poly-Si and a-Si: Difference between revisions

Kabi (talk | contribs)
Kabi (talk | contribs)
Line 53: Line 53:
'''Test wafer position:''' Center of the boat
'''Test wafer position:''' Center of the boat


A better uniformity of the resistivity across the wafer was achieved by subsequently annealing in N<sub>2</sub>, the annealing was done in Anneal Oxide Furnace (C1). Measured film thickness was 370 nm and the sheet resistance was measured to 200 &Omega;/sq +/- 15 &Omega;/sq.
A better uniformity of the resistivity across the wafer was achieved by subsequently annealing in N<sub>2</sub>, the annealing was done in Anneal Oxide Furnace (C1). The measured film thickness was 370 nm and the sheet resistance was measured to 200 &Omega;/sq +/- 15 &Omega;/sq.