| Line 52: | Line 52: | ||
'''Test wafer position:''' Center of the boat | '''Test wafer position:''' Center of the boat | ||
A better uniformity was achieved by annealing in N<sub>2</sub>. Measured film thickness was approximately 370 nm and the sheet resistance was measured to 200 | A better uniformity was achieved by annealing in N<sub>2</sub>. Measured film thickness was approximately 370 nm and the sheet resistance was measured to 200 &Omega/sq +/- 15 &Omega/sq. | ||