Specific Process Knowledge/Characterization/Lifetime scanner MDPmap: Difference between revisions
No edit summary |
|||
| Line 7: | Line 7: | ||
[[image:IMG_3290.jpg|400x400px|right|thumb|Lifetime scanner MPDmap, positioned in cleanroom D-3.]] | [[image:IMG_3290.jpg|400x400px|right|thumb|Lifetime scanner MPDmap, positioned in cleanroom D-3.]] | ||
== Microwave Detected Photoconductivity (MDP) == | |||
Topographic visualisation of electrically active defects or materiel properties at almost any production stage, allows for process optimization and performance prediction of devices. | |||
MDP is a contact less, non destructive measurement technology for the electrical characterization | |||
of a large variety of semiconductors. The mapping and visualization of so far not detectable | |||
defects was achieved by improving the sensitivity of a microwave detection system | |||
by several orders of magnitude. Electrical properties such as lifetime, τ, mobility, μ, and diffusion | |||
length, L, can be measured also at very low injection levels with a spatial resolution limited | |||
only by the diffusion length of the charge carriers. | |||
'''The user manual, control instruction, the user APV and contact information can be found in LabManager:''' | '''The user manual, control instruction, the user APV and contact information can be found in LabManager:''' | ||
Revision as of 12:31, 16 November 2015
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here

Microwave Detected Photoconductivity (MDP)
Topographic visualisation of electrically active defects or materiel properties at almost any production stage, allows for process optimization and performance prediction of devices.
MDP is a contact less, non destructive measurement technology for the electrical characterization of a large variety of semiconductors. The mapping and visualization of so far not detectable defects was achieved by improving the sensitivity of a microwave detection system by several orders of magnitude. Electrical properties such as lifetime, τ, mobility, μ, and diffusion length, L, can be measured also at very low injection levels with a spatial resolution limited only by the diffusion length of the charge carriers.
The user manual, control instruction, the user APV and contact information can be found in LabManager:
Lifetime scanner MPDmap info page in LabManager,
Performance information
| Equipment | Lifetime scanner MDPmap | |
|---|---|---|
| Purpose |
| |
| Location |
| |
| Performance | Resolution |
|
| Instrument specifics | Detector |
|
| Laser |
| |
| Substrates | Batch size |
|
| Allowed materials |
| |