Specific Process Knowledge/Characterization/Element analysis: Difference between revisions
Appearance
| Line 32: | Line 32: | ||
! style="background:WhiteSmoke; color:black" | What elements are detected | ! style="background:WhiteSmoke; color:black" | What elements are detected | ||
| style="background:WhiteSmoke; color:black" | Every element heavier than boron/carbon | | style="background:WhiteSmoke; color:black" | Every element heavier than boron/carbon | ||
| style="background:WhiteSmoke; color:black" | | | style="background:WhiteSmoke; color:black" | In principle every element, however, the sensitivity | ||
| style="background:WhiteSmoke; color:black" | Every element except hydrogen and helium. | | style="background:WhiteSmoke; color:black" | Every element except hydrogen and helium. | ||
|- | |- | ||
! style="background:lightgrey; color:black" | Chemical information | ! style="background:lightgrey; color:black" | Chemical information | ||
|style="background:lightgrey; color:black"| None | |style="background:lightgrey; color:black"| None | ||
|style="background:lightgrey; color:black"| None | |style="background:lightgrey; color:black"| None | ||
|style="background:lightgrey; color:black"| Chemical state information | |style="background:lightgrey; color:black"| Chemical state information | ||