Jump to content

Specific Process Knowledge/Lithography/EBeamLithographyManual: Difference between revisions

Tigre (talk | contribs)
Tigre (talk | contribs)
Line 395: Line 395:
|[[File:AGCRG2.png|400px]]
|[[File:AGCRG2.png|400px]]
|- align="center"
|- align="center"
| Open and edit AGCRG, in the program window <br> '''1'''Enter the measured (from pre-aligner output) P mark position '''2''' Click 'RG mark detect condition: Setting' and adjust scan width and position. Use a large scan width (200-600 microns). In 'Scan type' choose 'fine scan', 'box scan' and choose the correct mark (cross or L-shaped). Start with an 'X only' scan. '''3''' Save and execute AGCRG || blah blah 2
| Open and edit AGCRG, in the program window <br> '''1''' Enter the measured (from pre-aligner output) P mark position <br>'''2''' Click 'RG mark detect condition: Setting' and adjust scan width and position. Use a large scan width (200-600 microns). In 'Scan type' choose 'fine scan', 'box scan' and choose the correct mark (cross or L-shaped). Start with an 'X only' scan. <br>'''3''' Save and execute AGCRG || If the program finds the mark, ask the program to transfer the gain settings to SETWFR P (both rough and fine) or SETWFR Q. Scan again with same settings but choose 'Y only' in the 'RG mark detect conditions'.
|}
|}