| Line 404: | Line 404: | ||
*Enter the measured (from pre-aligner output) P mark position | *Enter the measured (from pre-aligner output) P mark position | ||
*Click 'RG mark detect condition: Setting' and adjust scan width and position. Use a large scan width (200-600 microns). In 'Scan type' choose 'fine scan', 'box scan' and choose the correct mark (cross or L-shaped). Start with an 'X only' scan. | *Click 'RG mark detect condition: Setting' and adjust scan width and position. Use a large scan width (200-600 microns). In 'Scan type' choose 'fine scan', 'box scan' and choose the correct mark (cross or L-shaped). Start with an 'X only' scan. | ||
*Save and execute AGCRG || If the program finds the mark, ask the program to transfer the gain settings to SETWFR P (both rough and fine) or SETWFR Q. Scan again with same settings but choose 'Y only' in the 'RG mark detect conditions'. | *Save and execute AGCRG ||If the program finds the mark, ask the program to transfer the gain settings to SETWFR P (both rough and fine) or SETWFR Q. Scan again with same settings but choose 'Y only' in the 'RG mark detect conditions'. | ||
|} | |} | ||