|98% Sulfuricacid and Ammoniumsulfat
|98% Sulfuricacid and Ammoniumsulfat
|98% Sulfuricacid and Hydrogenperoxide 4:1
|98% Sulfuricacid and Hydrogenperoxide 4:1 add H<math>_2</math>O<math>_2</math> to H<math>_2</math>SO<math>_4</math>
|-
|-
|'''Process temperature'''
|'''Process temperature'''
Line 29: Line 29:
|
|
10 min.
10 min.
|-
|'''Allowed materials'''
|
Dependent on which bath is used, look at the text in the pictures.
|
All materials (in beaker).
|-
|-
|'''Batch size'''
|'''Batch size'''

Revision as of 11:23, 21 February 2008

Cleaning of wafers or masks

Cleaning of wafers or masks with sulphuric acid can be done either in a dedicated tank "7-up" or in the fumehood in a beaker "Piranha" Both 7-up and Piranha removes heavy organics. Always use one of these after KOH to remove alkali ions before further processing. 7-up and Piranha are also used as cleaning solutions after stripping resist.

7-up Piranha
General description

Cleaning of wafers or masks using the dedicated tanks. There are one tank for masks and glasswafers and one for 4-6" Si wafers in cleanroom 4 and one tank in cleanroom 3 for 4" Si wafers only.

Cleaning of wafers using a beaker in the fumehood in cleanroom 2.Used for glass wafers or wafers with metal or other materials that you are not allowed to put in the 7-up for wafers.

Chemical solution 98% Sulfuricacid and Ammoniumsulfat 98% Sulfuricacid and Hydrogenperoxide 4:1 add H2O2 to H2SO4
Process temperature 80 oC ~70 oC the chemicals will heat up to working temperature during mixing, therefore be carefull!
Process time

10 min.

10 min.

Allowed materials

Dependent on which bath is used, look at the text in the pictures.

All materials (in beaker).

Batch size

1-19/25 4" wafers or 5 masks at a time

1-5 4" wafer at a time

Size of substrate

4-6" wafers

2-4" wafers