Specific Process Knowledge/Lithography/Coaters/Spin Coater: Gamma UV processing: Difference between revisions

Taran (talk | contribs)
Taran (talk | contribs)
Line 227: Line 227:


==AZ nLOF 2020 coating==
==AZ nLOF 2020 coating==
Spin coating of standard thicknesses (1.5 - 3 µm) of AZ nLOF 2020 on Spin Coater: Gamma UV is divided into two or three steps: HMDS priming (optional), spin coating, and soft baking. The HMDS priming is equal to the ''HMDS fast'' process. Spin coating uses dynamic dispense of resist at 800 rpm, using a volume of 3 ml for 100 mm substrates, and 5 ml for 150 mm substrates, respectively. The dispense is followed by spin-off at a thickness dependent spin speed for 30 seconds. The wafer is decelerated at 1000 rpm/s before stopping. Soft baking is done at 110°C for 60s.
Spin coating of standard thicknesses (1.5 - 3 µm) of AZ nLOF 2020 on Spin Coater: Gamma UV is divided into two or three steps: HMDS priming (optional), spin coating, and soft baking. The HMDS priming is equal to the ''HMDS fast'' process. Spin coating uses dynamic dispense of resist at 800 rpm, using a volume of 3 ml for 100 mm substrates, and 5 ml for 150 mm substrates, respectively. The dispense is followed by spin-off at a thickness dependent spin speed for 30 seconds. The wafer is decelerated at 2000 rpm/s before stopping. Soft baking is done at 110°C for 60s.


''Flow names, process parameters, and test results:''
''Flow names, process parameters, and test results:''