|'''General description'''
|'''General description'''
|
|
Cleaning of wafers or masks using the dedicated tanks. There are one tank for masks and pyrexwafers and one for 4-6" Si wafers in cleanroom 4 and one tank in cleanroom 3 for 4" wafers only.
Cleaning of wafers or masks using the dedicated tanks. There are one tank for masks and pyrexwafers and one for 4-6" Si wafers in cleanroom 4 and one tank in cleanroom 3 for 4" Si wafers only.
|
|
Cleaning of wafers using a beaker in the fumehood in cleanroom 2.Used for glass wafers or wafers with metal or other materials that you are not allowed to put in the 7-up for wafers.
Cleaning of wafers using a beaker in the fumehood in cleanroom 2.Used for glass wafers or wafers with metal or other materials that you are not allowed to put in the 7-up for wafers.