==Etching of Titanium==
Etching of Titanium is done wet at Danchip. We have two solutions for titanium etching:
 
{| border="2" cellspacing="0" cellpadding="4" align="left"
{| border="2" cellspacing="0" cellpadding="4" align="left"
!  
!  

Revision as of 15:11, 14 February 2008

Etching of Titanium

Etching of Titanium is done wet at Danchip. We have two solutions for titanium etching:

7-up Piranha
General description

Etch of pure Gold with or without photoresist mask.

Etch of pure Gold (as stripper).

Chemical solution KJ:J2:H2O (100g:25g:500ml) HCl:HNO3 (3:1)
Process temperature 20 oC 20 oC
Possible masking materials

Photoresist (1.5 µm AZ5214E)

Unmasked - used as a stripper

Etch rate

~100 nm/min

~(??) nm/min - fast etch

Batch size

1-5 4" wafers at a time

1-5 4" wafer at a time

Size of substrate

2-6" wafers

2-6" wafers