'''1 Material:''' Global marks or chip marks should be clearly visible in a 100keV SEM, i.e. preferably defined by Ti/Au or another 'heavy' metal, alternatively the wafer marks should be etched. | '''1 Material:''' Global marks or chip marks should be clearly visible in a 100keV SEM, i.e. preferably defined by Ti/Au or another 'heavy' metal, alternatively the wafer marks should be etched. Etched mark should be around 1 µm deep in order to be detectable by the machine; shallow etched (even 200 nm etched profiles) global marks or global marks defined by a light metal as Al can be hard to locate manually as well as automatically. | ||