|Sputter Coat
|Sputter Coat
|Cressington 208HR, DTU CEN
|Cressington 208HR, DTU CEN
|3-5 nm Pt, sputtering (29-08-2014 TIGRE)
|3-5 nm Pt, sputtering, please contact [mailto:ramona.mateiu@cen.dtu.dk Ramona Valentina Mateiu] for information (29-08-2014 TIGRE)
|3-5 nm Pt, sputtering (09-07-2014 TIGRE)
|3-5 nm Pt, sputtering (09-07-2014 TIGRE)
|3-5 nm Pt, sputtering (22-05-2014 TIGRE)