Line 16: Line 16:
! width="40" | Wafer ID
! width="40" | Wafer ID
! width="40" | Comments
! width="40" | Comments
|-
| 18/8-2014
| 4" Danchip QC Wafer
| 1.5 µm AZ resist, daq2 mask
| Si / 10 %
| Pegasus/jmli
| 10 minute TDESC clean, 10 minute PR strip post process
| danchip/QC/QCprocA, 55 cycles (11+44) or 10:05 minutes
| S004257
! OLD showerhead
|
[[file:S004257-08.jpg|150px|frameless ]]
[[file:S004257-09.jpg|150px|frameless ]]
[[file:S004257-10.jpg|150px|frameless ]]
[[file:S004257-11.jpg|150px|frameless ]]
[[file:S004257-12.jpg|150px|frameless ]]
[[file:S004257-13.jpg|150px|frameless ]]
[[file:S004257-14.jpg|150px|frameless ]]
|-
|}
{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;"
|+ '''Process runs'''
|-
! rowspan="2" width="40"| Date
! colspan="4" width="120"| Substrate Information
! colspan="4" | Process Information
! rowspan="2" width="500" |SEM Images
|-
! width="30" | Wafer info
! width="40" | Mask
! width="40" | Material/ Exposed area
! width="40" | Tool / Operator
! width="40" | Conditioning
! width="40" | Recipe
! width="40" | Wafer ID
! width="40" | Comments
|-
| 18/8-2014
| 4" Danchip QC Wafer
| 1.5 µm AZ resist, daq2 mask
| Si / 10 %
| Pegasus/jmli
| 10 minute TDESC clean, 10 minute PR strip post process
| danchip/QC/QCprocA, 55 cycles (11+44) or 10:05 minutes
| S004257
! OLD showerhead
|
[[file:S004257-08.jpg|150px|frameless ]]
[[file:S004257-09.jpg|150px|frameless ]]
[[file:S004257-10.jpg|150px|frameless ]]
[[file:S004257-11.jpg|150px|frameless ]]
[[file:S004257-12.jpg|150px|frameless ]]
[[file:S004257-13.jpg|150px|frameless ]]
[[file:S004257-14.jpg|150px|frameless ]]
|-
|-
| 1/12-2014
| 1/12-2014