Line 43: Line 43:
| danchip/showerhead/polySi etch DUV mask, 20 cycles or 3:02 minutes  
| danchip/showerhead/polySi etch DUV mask, 20 cycles or 3:02 minutes  
| S004675
| S004675
|
! New showerhead
|  
|  


|-
|-
|}
|}

Revision as of 14:33, 11 December 2014

Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
20/11-2014 6" Wafer with 210 nm oxide and 1800 nm polysilicon standard stepper mask (50 nm barc + 320 nm krf) Si / 50+ % Pegasus/jmli 10 minute TDESC clean + 45 sec barc etch danchip/showerhead/polySi etch DUV mask, 20 cycles or 3:02 minutes S004675 Old showerhead

1/12-2014 1/4 6" Wafer with 210 nm oxide and 1800 nm polysilicon crystalbonded on carrier standard stepper mask (50 nm barc + 320 nm krf) Si / 50+ % Pegasus/jmli 10 minute TDESC clean + 45 sec barc etch danchip/showerhead/polySi etch DUV mask, 20 cycles or 3:02 minutes S004675 New showerhead