! rowspan="2"| 15 minutes of black silicon recipe on blank wafer
! rowspan="2" width="100"| 15 minutes of black silicon recipe on blank wafer
| S004592
| S004592
| Wafer centre
| Wafer centre

Revision as of 13:07, 10 December 2014

Comparison of processes before and after the change of showerhead in December 2014
Process Before After
Wafer ID Comment SEM images Wafer ID Comment SEM images
15 minutes of black silicon recipe on blank wafer S004592 Wafer centre S004679 Wafer centre
S004592 Wafer edge S004679 Wafer edge