If your wafers are fragile or having thin membranes, cantilever or suspended bridges it can be a good idea to dry your wafers in the ethanol fume dryer.
If your wafers are fragile or having thin membranes, cantilevers or suspended bridges that risk to stick or adhere to the surface it can be a good idea to dry your wafers in the ethanol fume dryer. Ethanol is heated to 70°C and your wafers are placed in the fumes of Ethanol which will make the water to evaporate from the surface.