''If'' rinsing is used as well, the standard process is 60 seconds of rinse at 500 RPM, followed by 120/180 seconds of drying at 2000 RPM. | ''If'' rinsing is used as well, the standard process is 60 seconds of rinse at 500 RPM, followed by 120/180 seconds of drying at 2000 RPM. | ||
<gallery caption="Different places to dry your wafers" widths="200px" heights="200px" perrow=" | <gallery caption="Different places to dry your wafers" widths="200px" heights="200px" perrow="4"> | ||
image:spin-rinser-dryer-white.jpg|Image(s) of the equipment(s). | |||
image:spin-rinser-dryer-white.jpg|Image(s) of the equipment(s). | |||
image:spin-rinser-dryer-white.jpg|Image(s) of the equipment(s). | |||
image:spin-rinser-dryer-white.jpg|Image(s) of the equipment(s).</gallery> | |||
[[image:spin-rinser-dryer-white.jpg|200x200px|right|thumb|Image(s) of the equipment(s)]] | [[image:spin-rinser-dryer-white.jpg|200x200px|right|thumb|Image(s) of the equipment(s)]] | ||