Etching of chromium is done wet at Danchip making your own set up in a beaker in a | Etching of chromium is done wet at Danchip making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. We have two solution for this: | ||
# HNO<math>_3</math>:H<math>_2</math>O:cerisulphate - 90ml:1200ml:15g - standard at Danchip | # HNO<math>_3</math>:H<math>_2</math>O:cerisulphate - 90ml:1200ml:15g - standard at Danchip | ||
| Line 17: | Line 17: | ||
Etch of chromium | Etch of chromium | ||
| | | | ||
Etch of | Etch of chromium | ||
|- | |- | ||
|Chemical solution | |Chemical solution | ||