Jump to content

Specific Process Knowledge/Lithography/Development/Developer TMAH UV-lithography processing: Difference between revisions

Taran (talk | contribs)
Taran (talk | contribs)
Line 47: Line 47:
PEB: 60s @ 110°C
PEB: 60s @ 110°C


Development: SP 15-30s. For lift-off SP 30-60s
Development: SP 15-30s. For lift-off SP 60s (sidewall angle ~15°)
*'''AZ MiR 701'''
*'''AZ MiR 701'''
Exposure dose: ?
Exposure dose: ?