Jump to content

Specific Process Knowledge/Thermal Process/Oxidation/Wet oxidation C1 furnace: Difference between revisions

Paphol (talk | contribs)
Paphol (talk | contribs)
Line 89: Line 89:
'''Temperature:''' 1000, 1050, 1100 C
'''Temperature:''' 1000, 1050, 1100 C


'''Time:''' 0, 5, 15, 100, 180, 250, 360, 720 minutes
'''Growth Time:''' 0, 5, 15, 100, 180, 250, 360, 720 minutes


'''Steamer Flow Rate:''' 10 L/min
'''Steamer Flow Rate:''' 10 L/min