'''Temperature:''' 1000, 1050, 1100 C | '''Temperature:''' 1000, 1050, 1100 C | ||
'''Time:''' 15, 180, 360, 720 minutes | '''Growth Time:''' 15, 180, 360, 720 minutes | ||
'''Steamer Flow Rate:''' 10, 17.5, 25 L/min | '''Steamer Flow Rate:''' 10, 17.5, 25 L/min | ||