====Results (2)==== | ====Results (2)==== | ||
Figure 4 shows the oxide thickness as a function of oxidation time in three process temperatures. The oxide grows faster at the higher temperature. The prediction equations of each process temperature can be form by this plots. | Figure 4 shows the oxide thickness as a function of oxidation time in three process temperatures. The oxide grows faster at the higher temperature. The prediction equations of each process temperature can be form by this plots, which are based on this experiment in our specific furnaces and give more accurate results. [[media:Calculation_for_Wet_oxidation_for_Anneal_Oxide(C1).xlsx|'''Calculation for wet oxidation''']] | ||
''' | ''' | ||