====Experimental setup (2) Steamer flow rate has been fixed at 10 liter/minutes====
====Experimental setup (2) Steamer flow rate has been fixed at 10 liter/minutes====
'''
'''
The steamer flow rate has been fixed at 10liter per minutes. The test was done in difference growth time.       
The steamer flow rate has been fixed at 10 liter per minutes. The test was done in difference growth time.       


'''Pressure:'''  Atmosphere