'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DryEtchProcessing click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DryEtchProcessing click here]''' | ||
= | = Challenges and techniques common to all dry etch tools = | ||
This page contains information that is common to dry etch instruments. | |||
== Hardware and option comparison of the dry etchers at Danchip == | == Hardware and option comparison of the dry etchers at Danchip == | ||
The table below compares the hardware and the options. | |||