| Line 646: | Line 646: | ||
== Etch Tests == | == Etch Tests == | ||
The tests presented here are prelimenary results and this page will be updated regularly. I post this as the interest in etch resistance of CSAR is increasing; if you have wafers or chips you would like to have tested, please send me an | The tests presented here are prelimenary results and this page will be updated regularly. I post this as the interest in etch resistance of CSAR is increasing; if you have wafers or chips you would like to have tested, please send me an [[mailto:tigre@danchip.dtu.dk email]]. | ||