Line 33: Line 33:
* gas in chamber (Ar, N2, O2 or mixture).
* gas in chamber (Ar, N2, O2 or mixture).


In the tabel below ([[Sputtering rates]]) there a given a list of relative sputter rates for different materials (Al is set to 1).
In the tabel below ([[#Relative Sputter rates |Relative Sputter rates]]) there a given a list of relative sputter rates for different materials (Al is set to 1).
This means that You can estimate the sputter rate for a new material if you have the rate for another material under the same conditions.
This means that You can estimate the sputter rate for a new material if you have the rate for another material under the same conditions.
I think this only works for non-reactive sputtering (i.e. with Ar as the gas).