== Fluence definition ==  
== Fluence definition ==  


The fluence produces by a laser is, by definition, the energy delivered by a laser pulse (<math>E_{pulse}</math>) per surface unit (<math>S</math>) and it is given in J/cm2.  
The fluence produces by a laser is, by definition, the energy delivered by a laser pulse (<math>E_{pulse}</math>) per surface unit (<math>A</math>) and it is given in J/cm2.  





Revision as of 16:21, 26 May 2014

Fluence definition

The fluence produces by a laser is, by definition, the energy delivered by a laser pulse (Epulse) per surface unit (A) and it is given in J/cm2.


The function Epulse is defined as :


Epulse=P‾f

Where P‾ (average power) is measured with the laser sensor power measurement (see manual,section 5.3) and the repetion rate (f) is set in the parameter file under " laser frequency".

The fluence is therefore determinated as such :


Fluence=EpulseA

The area (A) can determinate with the theoretical min spot diameter (1/e2), available here

Fluence results measurement

Fluence result for IR wavelength (1064nm, F255mm)
Fluence result for green wavelength (532nm, F255mm)
Fluence result for UV wavelength (355nm, F255mm)