Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/fluence: Difference between revisions
Appearance
| Line 23: | Line 23: | ||
![[image:140414_FluenceVSrepRate_1064nm_255mm_v1.jpg|500x500px|thumb|center|Fluence result for IR wavelength (1064nm, F255mm)]] | ![[image:140414_FluenceVSrepRate_1064nm_255mm_v1.jpg|500x500px|thumb|center|Fluence result for IR wavelength (1064nm, F255mm)]] | ||
![[image:140414_FluenceVSrepRate_532nm_255mm_v1.jpg|500x500px|thumb|center|Fluence result for green wavelength (532nm, F255mm)]] | ![[image:140414_FluenceVSrepRate_532nm_255mm_v1.jpg|500x500px|thumb|center|Fluence result for green wavelength (532nm, F255mm)]] | ||
![[image:140526_FluenceVSrepRate_355nm_255mm_v1.jpg|500x500px|thumb|center|Fluence result for UV wavelength (532nm, F255mm)]] | |||
|} | |} | ||
Revision as of 14:43, 26 May 2014
Fluence definition
The fluence produces by a laser is, by definition, the energy delivered by a laser pulse () per surface unit () and it is given in J/cm2.
The function is defined as :
Where (average power) and is measured with the laser sensor power measurement (see manual,section 5.3) and the repetion rate () is set in the parameter file under " laser frequency".
The fluence is therefore determinate as such :
The theoretical spot sizes () can be found here