The theoretical spot sizes (<math>S</math>) can be found [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/Spot size and optics|here]] | The theoretical spot sizes (<math>S</math>) can be found [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/Spot size and optics|here]] | ||
== Fluence results measurement== | |||
{| border="1" cellspacing="2" cellpadding="2" | {| border="1" cellspacing="2" cellpadding="2" | ||
Revision as of 09:49, 12 May 2014
Fluence definition
The fluence produces by a laser is, by definition, the energy delivered by a laser pulse () per surface unit () and it is given in J/cm2.
The function is defined as :
Where (average power) and is measured with the laser sensor power measurement (see laser manual section 5.3) and the repetion rate () is set in the parameter file under " laser frequency".
The fluence is therefore determinate as such :
The theoretical spot sizes () can be found here