Jump to content

Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/fluence: Difference between revisions

From LabAdviser
Chasil (talk | contribs)
Chasil (talk | contribs)
Line 9: Line 9:
: <math>E_{pulse} = \frac{\overline{P}}{f}\,</math>
: <math>E_{pulse} = \frac{\overline{P}}{f}\,</math>


Where <math>\overline{P}</math> (average power) and is measured with the laser sensor power measurement and the repetion rate (<math>f</math>) is set in the settings.
Where <math>\overline{P}</math> (average power) and is measured with the laser sensor power measurement (see laser manual section 5.3) and the repetion rate (<math>f</math>) is set in the parameter file under " laser frequency".


The fluence is therefore determinate as such :  
The fluence is therefore determinate as such :  

Revision as of 09:40, 12 May 2014

Fluence

The fluence produces by a laser is, by definition, the energy delivered by a laser pulse (Epulse) per surface unit (S) and it is given in J/cm2.


The function Epulse is defined as :


Epulse=P‾f

Where P‾ (average power) and is measured with the laser sensor power measurement (see laser manual section 5.3) and the repetion rate (f) is set in the parameter file under " laser frequency".

The fluence is therefore determinate as such :


Fluence=EpulseS

The theoretical spot sizes (S) can be found here