| Line 5: | Line 5: | ||
The function <math>E_{pulse}</math> is defined as : | The function <math>E_{pulse}</math> is defined as : | ||
: <math>E_{pulse} = \frac{\overline{P}}{f}\,</math> | : <math>E_{pulse} = \frac{\overline{P}}{f}\,</math> | ||
Where (<math>\overline{P}</math>) is measured with the laser sensor power measurement and the repetion rate (<math>f</math>) is set in the settings. | Where (<math>\overline{P}</math>) is measured with the laser sensor power measurement and the repetion rate (<math>f</math>) is set in the settings. | ||
The fluence is therefore determinate as such : | |||
: <math>Fluence = \frac{E_{pulse}}{S}\,</math> | |||