Created page with "= Fluence = The fluence produces by a laser is by definition the energy delivered by a laser pulse per surface unit and it is given in J/cm2."
 
Chasil (talk | contribs)
No edit summary
Line 1: Line 1:
= Fluence =  
= Fluence =  


The fluence produces by a laser is by definition the energy delivered by a laser pulse per surface unit and it is given in J/cm2.
The fluence produces by a laser is, by definition, the energy delivered by a laser pulse (<math>E_{pulse}</math>) per surface unit (<math>E_{pulse}</math>) and it is given in J/cm2.
 
 
The function <math>E_{pulse}</math> is defined as :
 
: <math>E_{pulse} = \frac{\overline{P}}{f}\,</math>
 
Where (<math>\overline{P}</math>) is measured with the laser sensor power measurement and the repetion rate (<math>f</math>) is set in the settings.

Revision as of 11:50, 28 April 2014

Fluence

The fluence produces by a laser is, by definition, the energy delivered by a laser pulse (Epulse) per surface unit (Epulse) and it is given in J/cm2.


The function Epulse is defined as :

Epulse=P‾f

Where (P‾) is measured with the laser sensor power measurement and the repetion rate (f) is set in the settings.