The thickness is measured on VASE Ellipsometer using a simple Cauchy model for a transparent polymer on Si. The measurements are performed at one incidence angle (70 degrees) only. 9 points on each 4" wafer has been measured; the standard deviation thus representing the homogeinity of the film on the 4" wafers. | |||
{|border="1" cellspacing="0" cellpadding="3" style="text-align:left;" | {|border="1" cellspacing="0" cellpadding="3" style="text-align:left;" | ||