Deposition of Cu
Copper can be deposited by e-beam evaporation or sputtering . In the chart below you can compare the different deposition equipment.
Deposition of Copper using sputter deposition technique
E-beam evaporation (Alcatel) | Sputter deposition (PVD co-sputter/evaporation) | |
---|---|---|
General description | E-beam deposition of Cu | Sputter deposition of Cu |
Pre-clean | RF Ar clean | RF Ar clean |
Layer thickness | 10Å to 0.5µm* |
10Å to 1µm* |
Deposition rate | 2Å/s to 15Å/s |
Depending on process parameters |
Batch size |
|
|
Allowed materials |
|
|
Comment |
* To deposit layers thicker then 200 nm permission is required (contact Thin film group)
Studies of Cu deposition processes
Roughness of Cu layers - Roughness of Cu layers deposited with Alcatel