Jump to content

Specific Process Knowledge/Thin film deposition/Si sputter in Wordentec: Difference between revisions

From LabAdviser
Kn (talk | contribs)
No edit summary
Knil (talk | contribs)
No edit summary
Line 1: Line 1:
== Silicon sputter==
== Silicon sputter==


Silicon can be deposited in [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec.]]  
Silicon can be sputter deposited in [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec.]]  




Line 10: Line 10:




Please don´t use higher power then 180W, since the target then could breake into a lot of small pieces.
Please don´t use higher power then 180W, since the target then could break into a lot of small pieces.


{| border="1" cellspacing="0" cellpadding="4"  
{| border="1" cellspacing="0" cellpadding="4"  

Revision as of 09:07, 2 April 2014

Silicon sputter

Silicon can be sputter deposited in Wordentec.


Parameters

Listed below are tried parameters, that can be used during deposition. Use the rates as a start value, and make a test to be sure that you get the right thickness.


Please don´t use higher power then 180W, since the target then could break into a lot of small pieces.

Settings 1 Settings 2
Process type Sputtering Sputtering
Power 130W 170W
Sputter pressure 5*10-3 1*10-2
Rate About 0,7 Å/s About 0,6 Å/s