==Platinum deposition == | ==Platinum deposition == | ||
Platinum can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. | Platinum can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the different deposition equipment. | ||