!'''Allowed materials''' | !'''Allowed materials''' | ||
| | | | ||
*All wafers have to be RCA cleaned. | *All wafers have to be RCA cleaned. Except for Boron pre-dep wafer from furnace A1. | ||
| | | | ||
*All wafers have to be RCA cleaned. | *All wafers have to be RCA cleaned. | ||
| | | | ||
*All wafers have to be RCA cleaned. | *All wafers have to be RCA cleaned. Except for Phosphorous pre-dep wafers from furnace A4. | ||
| | | | ||
*All processed wafers have to be RCA cleaned. Except for wafers from LPCVD furnace and PECVD1. | |||
| | | | ||
*All wafers have to be RCA cleaned. Except for wafers from EVG-NIL and PECVD3. | |||
| | | | ||
| | | | ||