'''Wafers that go into the high temperature furnaces''' <br/>
'''Wafers that go into the high temperature furnaces''' <br/>
As a general rule all wafers that go into the high temperature furnaces need a full RCA clean directly before the furnace step. <br/>
As a general rule all wafers that go into the high temperature furnaces need a full RCA clean directly before the furnace step.  
<br/>


'''Wafers that have been in the KOH baths, KOH BHF baths or the warm phosphoric acid''' <br/>
'''Wafers that have been in the KOH baths, KOH BHF baths or the warm phosphoric acid''' <br/>